| Material |
Operating Temperature |
Insulation Resistance (I.R.) |
D.F. |
Test Surge Voltage |
Metallized
Mylar |
-55°C to +85°C
Derate linearly to 50% from +85°C to +125°C |
(50-100V) 10,000 Megohms/ mfd.
Not to exceed 40,000 Megohms
(200V + ) 25,000 Megohms/ mfd.
Not to exceed 60,000 Meg ohms |
< 1.0%
at 1 Khz
and at +25°C |
150%
of the rated Voltage |
| Mylar / Foil |
-55°C to +85°C
Derate linearly to 50% from +85°C to +125°C |
50,000 Megohms/ mfd.
Not to exceed 100,000 Megohms |
< 0.5%
at 1 Khz
and at +25°C |
200%
of the rated Voltage |
Metallized
Poly-
propylene |
-55°C to +85°C
Derate linearly to 60% from +85°C to +105°C |
200,000 Megohms/ mfd.
Not to exceed 400,000 Megohms |
< 0.2%
at 1 Khz
and at +25°C |
150%
of the rated Voltage |
Poly-
propylene / Foil |
-55°C to +85°C |
250,000 Megohms/ mfd.
Not to exceed 500,000 Megohms |
< 0.1%at 1 Khz and at +25°C |
200%
of the rated Voltage |
| Mylar / Kraft / Foil |
-55°C to +85°C
Derate linearly to 60% from +85°C to +125°C |
20,000 Megohms/ mfd.
Not to exceed 100,000 Megohms |
< 1.0%
at 1 Khz
and at +25°C |
200%
of the rated Voltage |
*Metallized
Poly-
phenylene Sulfide |
-55°C to +125°C |
(50-100V) 25,000 Megohms/ mfd.
Not to exceed 50,000 Megohms
(200V + ) 50,000 Megohms / mfd.
Not to exceed 100,000 Megohms |
< 0.15%
at 1 Khz
and at +25°C |
150%
of the rated Voltage |
*Poly-
phenylene Sulfide / Foil |
-55°C to +125°C |
100,000 Megohms/ mfd.
Not to exceed 200,000 Megohms |
< 0.15%
at 1 Khz
and at +25°C |
200%
of the rated Voltage |
** Metallized Poly-
carbonate |
-55°C to +125°C |
(50-100V) 25,000 Megohms/ mfd.
Not to exceed 50,000 Megohms
(200V + ) 50,000 Megohms/ mfd.
Not to exceed 100,000 Megohms |
< 0.30%
at 1 Khz
and at +25°C |
150%
of the rated Voltage |
| Teflon / Foil |
-55°C to +150°C |
250,000 Megohms /mfd.
Not to exceed 500,000 Megohms |
< 0.2% @ 1 khz
and at +25°C |
200% of rated Voltage |